Quote:
Originally Posted by mkart View Post
Do you use Weld On 1001 to bond the two materials together? I remember the first time I made a calcium reactor I used the wrong glue and spider cracked the acrylic. I have been looking at the Red Sea, Geo and Deltec sumps for ideas. Need to call Regal Plastics for a quote. Great idea on the white PVC versus white acrylic. I assume it’s cheaper.


Sent from my iPhone using Tapatalk


I mix my own chemicals. It’s mostly methylene chloride and some thickener. 100 to 5 ratio. This actually melts the two plastics together like weld on instead of just flying them.

There are many reasons for crazing. The most common are because the use of alcohol based bonding agents or because the edges were overheated when cutting.


Sent from my iPhone using Tapatalk


__________________
"The only thing that interferes with my learning is my education."

Albert Einstein

Current Tank Info: 110 Gal Display, 125 Gal Custom Sump in basement fish room, 2- G3 XR30 Radion's + 2 48' Retrofit T5"s, Super Reef Octopus XP 2000 SSS Skimmer, 2 - Vortech MP-40, Panworld NH-200PS Return, 8x2' Frag tank, DIY refugium lighting, DIY frag tank lighting.
Schplitter is offline   Reply With Quote